Homogenization heat treatment of cast superalloy 718Plus - an investigation of the microstructural evolution upon heat treatment
- Författare
- Josefin E. C. Larsson
- (Josefin E. C. Larsson., Examensarbete, Diploma work in the Master programme Advanced Engineering Materials)
- Genre
- Ej skönlitteratur
- Språk
- Engelska
| Förlag | År | Ort | Om boken | ISBN |
|---|---|---|---|---|
| Chalmers University of Technology | 2009 | Sverige, Göteborg | vi, 53, 21 sidor. ill. |